Neoprene rubber US main models

by Dongrubber on December 13, 2006 · 0 comments

Model Grade Mooney viscosityML(1+4)100℃ Features Crystallization rate
 

G

GNGNA 50~6242~59 general typesuperior raw rubber stability MediumMedium
GW 26~54 Properties combined G & W type, no need for peptizer slow
GRTGK

FB

30~45(be liquid at 55℃) Anti high crystallization/ adhesion typeGW type

processing agent can vulcanize, non-volatile

Slow 

Slow

 

 

 

 

 

 

 

 

 

W

W 40~49 general type Quick
WM-1NPG6206 34~4240~50 Low viscosity W typeQuick vulcanizing rate, enhanced physical property W type QuickQuick
WHVWB 106~12543~52 High viscosity W typeContain gel, easy to process QuickMedium
NPR9503NPR9327

WRX

WRT

WRT-M1

70~9045~55

42~51

41~51

34~42

Few moulds pollution typeGood flexible resistance

GRT that anti crystallization

Maximum anti crystallization property

Low viscosity WRT

Slow 

Slow

Slow

 

Very slow

Very slow

WDWK 100~12048~79 High viscosity WRTIdeal anti collapse property Very slowVery slow
 

T

TW 42~52 Better processing property than W Quick
W-100 85~102 Higher viscosity TW type Quick
TRT 42~52 Better processing property than WRT Very slow